Dedicated to EYSF-021 surface chemistry of titanium and titanium alloy polishing, and effectively remove the surface of titanium oxide.
Usage:
1, pre-polishing to ensure that the titanium surface without oil and other materials沾附. 2, liquid use, please do not dilute. 3, temperature 10-35 ℃. 4, polishing time for 5-30 seconds (depending on the degree of oxidation). 5, polished finish quickly clean water. 6, the use of appropriate protective measures to avoid further oxidation.
Note:
1, strong corrosive substances, and pay attention to protection. 2, inhalation of harmful to health, to keep the workplace ventilation. 3, once touched on the skin or splashing into eyes, rinse immediately with plenty of water, such as burning sensation occur, seek medical treatment immediately. 4, after the discharge of treated residue. 5,勿使of reach of children. 6, Honey closure to preserve the shade. |