YSC-338 in addition to wax is a high-performance water to remove dirt of all kinds of outstanding gatch polished metal products prior to treatment. It has the following characteristics:
1, infiltration, dissolution and strong, with the exception of wax efficient, fast.
2, does not contain sodium hydroxide and inorganic salt, alkaline is extremely rare.
3, the use of low concentrations (1-3%), high capacity of oil, long life, the economy.
4, applies to a wide range of - alloys (containing zinc, magnesium, aluminum alloy), steel, iron treatment of wax in addition to, the following type: strap, watch cases, jewelry, alloy fittings, glasses and other lighting products are applicable.
Use and maintenance
Weight :10-30 ml / L
Temperature: Hot-dip 60-90 ℃, ultrasonic washing 60-80 ℃
1-10-minute time
The use of the main points:
1, solution preparation: First, add water into the well-ching tank, heated to about 60 ℃, under stirring at slowly add the necessary wax YSC-338 in addition to water.
2, solution maintenance: In addition to the wax solution performance and speed can be calculated through the use of chemicals or to use their experience to add in addition to water to maintain the wax so that the final wax or oil pollution when too many solids, the solution need to be replaced.
3, For a slot with the same quality for a number of different matrix in addition to wax, it is necessary to pay attention to the order in addition to wax, lively metal first, and then again less active metal. For example: In addition to the first wax to zinc alloy, followed by copper and its alloys do. Not recommended for a large number of copper or its alloy and then again after the zinc alloy, zinc alloy or at the surface of items in addition to the formation of a layer of wax combined with poor copper replacement.